Skip to content

7075 Aluminum Alloy

EN AW-7075

Available on Request

  • ENEN AW-7075
  • ENAlZn5,5MgCu
  • DIN3.4365
  • UNSA97075

EN AW-7075 (AlZn5,5MgCu, UNS A97075) is a high-strength zinc-magnesium-copper aluminum alloy hardened by solution treatment and artificial ageing. T6 / T651 gives high strength, while T73 / T7351 offers better resistance to stress corrosion cracking. Supplied to specification as plate and bar for aerospace, defense and mold applications.

Spectral Analysis

wt. % · EN 573-3 ranges
Al
balance
Zn
5.1–6.1
Mg
2.1–2.9
Cu
1.2–2.0
Cr
0.18–0.28
Si
≤0.40
Fe
≤0.50
Mn
≤0.30
Ti
≤0.20

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rm ≈ 540–570 MPa, Rp0.2 ≈ 470–505 MPa (T6 / T651, thickness dependent, typical)
  • Rm ≈ 470–505 MPa, Rp0.2 ≈ 390–435 MPa (T7351, typical)
  • Hardness ≈ 150 HB (T6)
  • Density ≈ 2.81 g/cm³
  • In T6, thick sections are susceptible to stress corrosion in the short transverse direction; T73 tempers are preferred for this reason
  • Good machinability; not suited to fusion welding

02Applications

  • Aerospace structural parts (wing and fuselage fittings)
  • Defense components
  • Blow molds and plastic prototype molds
  • Highly loaded machine and fixture parts
  • Bicycles, sports equipment and climbing hardware

03Delivery Condition

  • T6 / T651: solution treated and artificially aged; T651 plate stress relieved by stretching.
  • T73 / T7351: overaged; for stress corrosion resistance.
  • T6511 / T73511: extrusions and bar.
  • O: annealed, on request.
  • Standards: EN 485 / EN 755, ASTM B209 / B211 / B221, AMS (QQ-A-250/12 equivalents).

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →465–480 °C

Quench: Water

AgeingTemperatureTime →~120 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are typical and vary with temper and thickness. The diagram shows T6 ageing.

05Is there a better material?

Grades in the same material family as 7075 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than 7075 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Plate
  • Sheet
  • Round bar
  • Flat bar
  • Extrusions
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 (on request, third party)
  • Tensile and hardness testing (temper verification)
  • Temper verification by electrical conductivity (e.g. AMS 2658)
  • Ultrasonic testing (thick plate; e.g. ASTM B594 / AMS-STD-2154)

Supply status: Available on Request

Request 7075 Quotation

Not sure if 7075 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote