Skip to content

Inconel • Hastelloy • Nickel-Based Alloys

Nickel Alloys & Superalloys

Inconel and Hastelloy supplier in Turkey through international sourcing. High-performance nickel-based alloys for applications operating under high temperature, corrosion and mechanical load. International sourcing according to specification and quantity.

Search Nickel Alloys & Superalloys by grade or standard (e.g. Alloy 625, Alloy 718, Alloy 600). If there is no match, your request goes straight to the quote form.

Enter: open the matching page, otherwise open the quote form

01

Overview

Nickel alloys are alloys in which nickel is the main element or, together with iron, forms the basis of the structure; additions of chromium, molybdenum, iron, copper, cobalt, niobium, titanium and aluminium produce different property profiles. They are broadly classified as corrosion-resistant alloys (Ni-Cr-Mo, Ni-Mo, Ni-Cu), high-temperature alloys (Ni-Cr, Ni-Fe-Cr), age-hardenable superalloys and controlled-expansion alloys. Their austenitic structure retains toughness at low and high temperatures; superalloys gain high-temperature strength through γ′ and γ″ precipitates. Selection weighs service temperature, environment (oxidising or reducing, chlorides, H₂S), load and duration, together with the applicable specification.

  • Ni-Cr-Mo (625, C-276, C-22): resistance to pitting and crevice corrosion in chloride and acidic media
  • Ni-Mo (B-2, B-3): corrosion resistance in reducing acids such as hydrochloric acid
  • Ni-Cu (400, K-500): seawater and hydrofluoric acid environments
  • Age-hardenable (718, X-750, Waspaloy): high-temperature strength through γ′ / γ″ precipitates
  • Ni-Fe-Cr (800H, 825): high-temperature and general corrosion service with lower nickel content
  • Invar 36 and Kovar: controlled thermal expansion

02

Material Grades

02.1

Inconel Alloys

Nickel-chromium alloys (600, 601, 625, 718, X-750 etc.); strength, oxidation and corrosion resistance at high temperature. Selection depends on temperature, load, duration and environment.

Typical applicationsGas turbine and engine parts, heat-treatment furnace equipment, aerospace, energy and chemical processing.

02.2

Hastelloy Alloys

Nickel-molybdenum and nickel-chromium-molybdenum alloys (C-276, C-22, C-4, B-2, B-3) provide corrosion resistance in acidic and chloride environments; oxidising versus reducing conditions drive the selection. Hastelloy X (Ni-Cr-Fe-Mo) is used for oxidation resistance and strength at high temperature.

Typical applicationsChemical and petrochemical processing, flue gas desulphurisation, acid production, heat exchangers; gas turbine combustor and furnace parts for Hastelloy X.

02.4

Other Nickel Alloys & Superalloys

Incoloy 800H and 825, Nimonic 80A, Waspaloy, commercially pure nickel (Alloy 200) and the controlled-expansion alloys Invar 36 and Kovar.

Typical applicationsHigh-temperature and turbine parts, petrochemical, electronics and precision measurement applications.

03

Chemical Composition

GradeNiCrMoFeCoCuNb+TaTiAl
Inconel Alloys
Alloy 625 (Inconel 625) Nickel Alloy≥58.020.0–23.08.0–10.0≤5.0——3.15–4.15≤0.40≤0.40
Alloy 718 (Inconel 718) Nickel Alloy50.0–55.017.0–21.02.80–3.30balance——4.75–5.500.65–1.150.20–0.80
Alloy 600 (Inconel 600) Nickel Alloy≥72.014.0–17.0—6.0–10.0—————
Alloy 601 (Inconel 601) Nickel Alloy58.0–63.021.0–25.0—balance————1.00–1.70
Alloy X-750 (Inconel X-750) Nickel Alloy≥70.014.0–17.0—5.0–9.0——0.70–1.202.25–2.750.40–1.00
Alloy 690 (Inconel 690) Nickel-Chromium-Iron Alloy≥58.027.0–31.0—7.0–11.0—≤0.50———
Alloy 706 (Inconel 706) Nickel-Iron-Chromium Superalloy39.0–44.014.5–17.5—balance——2.5–3.31.5–2.0≤0.40
Alloy 725 (Inconel 725) Nickel Alloy55.0–59.019.0–22.57.0–9.5balance——2.75–4.01.0–1.7≤0.35
Hastelloy Alloys
Alloy C-276 (Hastelloy C-276) Nickel Alloybalance14.5–16.515.0–17.04.0–7.0≤2.5————
Alloy C-22 (Hastelloy C-22) Nickel Alloybalance20.0–22.512.5–14.52.0–6.0≤2.5————
Alloy B-2 (Hastelloy B-2) Nickel-Molybdenum Alloybalance≤1.026.0–30.0≤2.0≤1.0————
Alloy C-4 (Hastelloy C-4) Nickel-Chromium-Molybdenum Alloybalance14.0–18.014.0–17.0≤3.0≤2.0——≤0.70—
Alloy B-3 (Hastelloy B-3) Nickel-Molybdenum Alloy≥65.01.0–3.027.0–32.01.0–3.0—————
Alloy X (Hastelloy X) Nickel-Chromium-Iron-Molybdenum Alloybalance20.5–23.08.0–10.017.0–20.00.50–2.50————
Monel Alloys
Alloy 400 (Monel 400) Nickel-Copper Alloy≥63.0——≤2.5—28.0–34.0———
Alloy K-500 (Monel K-500) Nickel-Copper Alloy≥63.0——≤2.0—27.0–33.0—0.35–0.852.30–3.15
Other Nickel Alloys & Superalloys
Alloy 800H / 800HT (Incoloy) Nickel-Iron-Chromium Alloy30.0–35.019.0–23.0—≥39.5—————
Alloy 825 (Incoloy 825) Nickel-Iron-Chromium Alloy38.0–46.019.5–23.52.5–3.5≥22.0—1.5–3.0—0.6–1.2—
Waspaloy Nickel-Base Superalloybalance18.0–21.03.5–5.0≤2.012.0–15.0——2.75–3.251.20–1.60
Nimonic 80A Nickel-Chromium Superalloybalance18.0–21.0—≤3.0≤2.0——1.80–2.701.00–1.80
Nickel 200 / 201 Commercially Pure Nickel≥99.0——≤0.40—≤0.25———
Invar 36 Low-Expansion Nickel-Iron Alloy35.0–37.0——balance—————
Kovar (ASTM F15) Glass-Sealing Nickel-Cobalt-Iron Alloy29.0——balance17.0————
Alloy 20 (Carpenter 20Cb-3) Nickel-Iron-Chromium Alloy32.0–38.019.0–21.02.0–3.0balance—3.0–4.08×C–1.00——

Values in wt. %; ranges per each grade’s reference standard. The full list and reference standard are on the grade page. The analysis on the material certificate governs on delivery.

04

Mechanical Properties

Values for bar products are minimum (≥) values from the relevant ASTM / AMS specifications or typical (≈) values; they vary with delivery and heat-treatment condition and section size. For age-hardenable alloys, values depend on the solution and ageing cycle applied.

GradeConditionTensile strength Rm (MPa)Yield strength Rp0.2 (MPa)Elongation A (%)Hardness
Alloy 600Annealed (ASTM B166)≥ 550≥ 240≥ 30—
Alloy 625Annealed, Grade 1 (ASTM B446, ≤ 100 mm)≥ 827≥ 414≥ 30—
Alloy 718Solution treated + aged (AMS 5663)≥ 1275≥ 1034≥ 12≈ 40–45 HRC
Alloy C-276Solution annealed (ASTM B574)≥ 690≥ 283≥ 40—
Alloy C-22Annealed (ASTM B574)≥ 690≥ 310≥ 45—
Alloy 400Annealed (ASTM B164)≥ 483≥ 172≥ 35—
Alloy K-500Aged (typical)≈ 950–1100——≈ 27–35 HRC
Alloy 825Annealed (ASTM B425)≥ 586≥ 241≥ 30—
Alloy 800H / 800HTSolution annealed (ASTM B408)≥ 448≥ 172≥ 30—
WaspaloySolution treated + stabilised + aged (typical)≈ 1250–1400——≈ 36–42 HRC

For information only. Sheet, plate, tube and forgings are covered by different specifications and values. The applicable specification and material certificate govern every order.

05

Physical Properties

Approximate room-temperature values; representative grades are shown to illustrate the differences between alloy families.

Grade / groupDensity (g/cm³)Modulus of elasticity (GPa)Thermal conductivity (W/m·K)Thermal expansion coefficient (10⁻⁶/K, 20–100 °C)
Alloy 6008.4720714.913.3
Alloy 6258.442079.812.8
Alloy 7188.1920011.413.0
Alloy C-2768.89205≈ 1011.2
Alloy 4008.8018021.813.9
Alloy 8258.1419611.114.0
Invar 368.1141≈ 10≈ 1.3

Values are approximate; thermal expansion values refer to roughly 20–100 °C. Use producer data and the material certificate for design calculations.

06

Applications

  • Aerospace: gas turbine discs, shafts, blades and fasteners (718, Waspaloy)
  • Energy: turbine parts, heat exchangers and steam generator tubing (690)
  • Chemical and petrochemical: reactors, columns and piping (C-276, C-22, 825)
  • Oil and gas: downhole equipment, valves and fasteners (718, 725, 625)
  • Marine: pump shafts, valve parts and seawater equipment (400, K-500)
  • Heat treatment and furnace equipment: muffles, baskets and radiant tubes (600, 601, 800H)
  • Environmental technology: flue gas desulphurisation and acid production (C-276, C-22)
  • Electronics and precision measurement: glass-to-metal seals and low-expansion parts (Kovar, Invar 36)
  • Defense: components requiring high-temperature and corrosion resistance

07

Product Forms & Delivery Conditions

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Availability depends on alloy, specification and quantity.

Delivery conditions

  • Annealed — e.g. Alloy 600, 625 Grade 1, 400, 825
  • Solution annealed — e.g. C-276, 625 Grade 2, 800H / 800HT
  • Solution treated, ready for ageing — e.g. 718, X-750, Waspaloy, K-500
  • Solution treated + aged (e.g. AMS 5663)
  • Stress relieved (upon request)
  • Hot rolled or forged, cold drawn; peeled or ground surface

08

Applicable Standards & Certification

Product standards and specifications

  • ASTM B166 — Ni-Cr-Fe alloys (600, 601, 690) rod, bar and wire
  • ASTM B446 — Ni-Cr-Mo-Nb alloy (625) rod and bar
  • ASTM B637 — Precipitation-hardening nickel alloy bars and forgings (718, X-750, Waspaloy)
  • ASTM B574 / B335 — Ni-Cr-Mo (C-276, C-22, C-4) and Ni-Mo (B-2, B-3) rod
  • ASTM B164 / B865 — Ni-Cu alloys (400 / K-500) rod and bar
  • ASTM B408 / B425 — Ni-Fe-Cr (800H) and Ni-Fe-Cr-Mo-Cu (825) rod and bar
  • ASTM B168 / B443 / B575 — 600, 625 and Ni-Cr-Mo alloys plate, sheet and strip
  • AMS 5662 / AMS 5663 — Alloy 718 bars and forgings (solution treated / aged)
  • AMS 5666 (625), AMS 5667 (X-750), AMS 5706 / 5707 (Waspaloy) — aerospace specifications
  • NACE MR0175 / ISO 15156 — Material requirements for H₂S-containing oil and gas environments

Certification and inspection documents

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)
  • PMI (positive material identification)
  • Heat-treatment report, tensile and hardness test results

A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.

Hard-to-find nickel alloys?

Send us your specification and quantity. We review grade, standard, dimensions, heat-treatment condition, testing and certification requirements together and identify suitable options through our international supplier network.

Material Availability & Supply Capability

Move Metal is not a producer; we focus on technical supply and international sourcing. The supply status of each grade is shown with the statuses below; a grade listed on the site does not mean it is held in stock.

Regular Supply
Materials with an established supply relationship, available for recurring requirements.
Available on Request
Materials sourced on request through our international producer and supplier network.
Special Sourcing
Requirements calling for special dimensions, certification or producer approval, sourced individually.
Under Development
Materials we are working to bring into our supply scope.

Please Include

  • Alloy (with UNS or W.Nr.)
  • Standard and specification (e.g. ASTM B446, AMS 5662)
  • Dimensions and tolerance
  • Heat-treatment condition (annealed, solution treated, aged)
  • Testing requirements
  • Certification
  • Origin
  • Quantity

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote