Skip to content

Alloy 625 (Inconel 625) Nickel Alloy

Alloy 625

Sourced upon request

  • EN2.4856
  • ENNiCr22Mo9Nb
  • UNSN06625
  • TicariInconel® 625

Nickel-chromium-molybdenum-niobium solid-solution alloy. Combines high corrosion resistance in chloride media, acids and seawater with strength up to 980 °C; good weldability. Sourced to specification.

01Material Properties

  • High resistance to pitting and crevice corrosion
  • Service from cryogenic to 980 °C
  • Not hardenable by heat treatment; solid-solution strengthened
  • Excellent weldability
  • High fatigue and thermal fatigue strength

02Applications

  • Chemical and petrochemical process equipment
  • Marine and offshore components
  • Gas turbine exhaust and combustion parts
  • Flue gas desulphurisation systems
  • Weld overlay and filler

03Delivery Condition

  • Annealed (Grade 1) or solution annealed (Grade 2); bar, plate, sheet, tube.

04Heat Treatment

Typical values

Annealing (Grade 1)
870–1040 °C; rapid cooling
Solution annealing (Grade 2)
1095–1205 °C; water
Hardening
Not hardenable by heat treatment
Stress relieving
Normally not required
Post-weld
No heat treatment required

Heat treatment cycle (schematic)

02004006008001000Anneal980°1. Anneal — 980 °C2. Quench — 25 °CTime (schematic, not to scale)°C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.