Nickel 200 / 201 Commercially Pure Nickel
Alloy 200 / 201
Available on Request
- UNSN02200 / N02201
- EN2.4066 / 2.4068
- ENNi 99.2 / LC-Ni 99
- TicariNickel 200 / 201
Commercially pure nickel with at least 99 % Ni; grade 201, with reduced carbon, is selected for service above 315 °C. Resistant to caustic soda and alkalis and a good conductor of heat and electricity, it is used in caustic plants, food processing and electronic parts.
Spectral Analysis
wt. % · ASTM B160 ranges- Ni
- ≥99.0
- Fe
- ≤0.40
- Mn
- ≤0.35
- Cu
- ≤0.25
- Si
- ≤0.35
- C
- ≤0.15 (200) / ≤0.02 (201)
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- Outstanding resistance in caustic soda and alkalis
- Good thermal and electrical conductivity
- Ferromagnetic (Curie ≈ 360 °C)
- 201: low carbon for service above 315 °C
- Very good formability and weldability
- Not hardenable by heat treatment; strength by cold work
02Applications
- Caustic soda production and storage equipment
- Food processing equipment
- Electronic and electrical parts, anodes
- Chemical vessels and containers
- Magnetostrictive devices and salt production equipment
03Delivery Condition
- Annealed; bar, plate, sheet, strip, tube, wire (ASTM B160 / B162 / B161).
04Please Include in Your Request
- Standard and delivery condition
- Form and dimensions (bar, plate, sheet, tube, forging)
- Quantity
- Testing and certification (EN 10204 3.1 / 3.2, NACE)
- Origin requirements
05Heat Treatment
Heat Treatment Steps
Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.
06Is there a better material?
Grades in the same material family as Nickel 200 / 201 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
Our list has no grade with higher wear resistance than Nickel 200 / 201 without a marked trade-off in its other critical properties.
Higher impact resistance (toughness)
Our list has no grade with higher impact resistance (toughness) than Nickel 200 / 201 without a marked trade-off in its other critical properties.
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights07Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Plate
- Sheet
- Tube
- Forgings
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 inspection certificate (upon request, third party)
- Ultrasonic testing (e.g. ASTM E2375), upon request
- Intergranular corrosion testing (e.g. ASTM G28)
- Grain size report (ASTM E112)
Supply status: Available on Request
Request Nickel 200 / 201 QuotationNot sure if Nickel 200 / 201 is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialTechnical resources for this material
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.