Skip to content

100Cr6 (52100) Bearing Steel

1.3505

Available on Request

  • EN1.3505
  • EN100Cr6
  • AISI52100
  • UNSG52986

High-carbon (0.93–1.05 %), 1.5 % chromium through-hardening bearing steel (100Cr6, AISI 52100). Hardening and low-temperature tempering bring it to 60–64 HRC with high rolling contact fatigue and wear resistance. Supplied to specification in the spheroidise-annealed condition for bearing parts, bushings and precision shafts.

Spectral Analysis

wt. % · EN ISO 683-17 ranges
C
0.93–1.05
Si
0.15–0.35
Mn
0.25–0.45
Cr
1.35–1.60
Mo
≤0.10

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • 60–64 HRC after hardening
  • High rolling contact fatigue strength
  • High wear resistance
  • Good machinability in the spheroidise-annealed condition
  • Hardenability is limited in larger sections; Mo-bearing variants are considered there

02Applications

  • Bearing rings, balls and rollers
  • Linear guide shafts and bushings
  • Precision shafts and pins
  • Gauges and measuring tools
  • Small punches and cold forming parts

03Delivery Condition

  • Spheroidise annealed (+AC), max. 207 HB; bar, tube or wire.

04Heat Treatment

Heat Treatment Steps

HardeningTemperatureTime →Austenitise830–870 °C
TemperingTemperatureTime →150–180 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 65 HRC150 °C → 63 HRC200 °C → 61 HRC250 °C → 59 HRC300 °C → 57 HRC400 °C → 52 HRC500 °C → 46 HRC600 °C → 38 HRC010020030040050060030354045505560657075Tempering temperature [°C]Hardness [HRC]1.3505Heat treatment: 830–870 °C
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 100Cr6 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than 100Cr6 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Peeled bar
  • Ground shafting
  • Hexagon
  • Flat bar
  • Plate
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, mechanical tests)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Tensile and impact (Charpy KV) test report
  • Jominy end-quench test (EN ISO 642) report
  • Ultrasonic testing (e.g. EN 10308 for bars, EN 10228-3 for forgings)

Supply status: Available on Request

Request 100Cr6 Quotation

Not sure if 100Cr6 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote