16NiCrMo12 Case-Hardening Steel

16NiCrMo12

Available on Request

  • UNI16NiCrMo12
  • EN~14NiCrMo13-4 (yakın)
  • EN~1.6657 (yakın)
  • AFNOR~16NCD13

Case-hardening steel with 2.70–3.20 % nickel, chromium and molybdenum (UNI 7846: 16NiCrMo12). The closest EN grade is 14NiCrMo13-4 (1.6657), but the compositions are not identical. After carburising it combines a hard case with a tough, strong core thanks to its high nickel content; supplied annealed on request for highly loaded gears and rolling elements.

Spectral Analysis

wt. % · UNI 7846 ranges
C
0.13–0.19
Si
0.15–0.40
Mn
0.40–0.70
Cr
0.80–1.10
Mo
0.30–0.40
Ni
2.70–3.20

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Surface hardness ≈ 62–64 HRC after carburising (tempering 150–200 °C)
  • Core Rm ≈ 980–1520 MPa (depending on section)
  • High hardenability; medium and large sections
  • Very good core toughness through high nickel
  • High surface fatigue (pitting) and impact resistance
  • Differs from 14NiCrMo13-4: lower nickel (2.70–3.20 %), higher molybdenum (0.30–0.40 %)

02Applications

  • Highly loaded gears and pinions
  • Rolling elements and highly loaded bearing parts
  • Gearbox and driveline components
  • Shafts and pins under impact loading
  • Motorsport, defence and heavy machinery driveline parts

03Delivery Condition

  • Soft annealed (+A, max. 250 HB) or isothermally annealed (+I, 190–236 HB); bar and forgings.
  • Where material is ordered under the UNI name, supply as EN 14NiCrMo13-4 (1.6657) is assessed against composition and specification.

04Heat Treatment

Heat Treatment Steps

CarburisingTemperatureTime →870–900 °C
HardeningTemperatureTime →Austenitise~795 °C
TemperingTemperatureTime →150–200 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

100 °C → 64.5 HRC150 °C → 64 HRC200 °C → 62 HRC250 °C → 59 HRC300 °C → 57 HRC0100200300400505560657075Tempering temperature [°C]Hardness [HRC]
Surface hardness after carburising versus tempering temperature (approximate, producer data).

If welding is required, it is done in the annealed condition and before carburising, with 150–350 °C preheating. Values are typical (producer data); the applicable specification governs for orders.

05Mechanical Properties

Delivery hardness and test-bar values after core hardening + stress relieving (UNI 7846, reference); core strength depends on section size.

ConditionSection (mm)Rm (MPa)Rp0.2 min. (MPa)Hardness
Soft annealed (+A)All——Max. 250 HB
Isothermally annealed (+I)All——190–236 HB
Core hardened + stress relieved111230–1520980363–432 HB
Core hardened + stress relieved301080–1370785327–394 HB
Core hardened + stress relieved63980–1270735295–373 HB
Carburised + hardened + tempered — surface———≈ 62–64 HRC

Reference values for UNI 7846 test bars (producer data; the 30 and 63 mm rows are for information). The applicable specification and material certificate govern for orders.

06Applicable Standards & Specifications

  • UNI 7846 — Case-hardening steels (16NiCrMo12; former Italian standard, still used as a reference)
  • EN 10084 — Case-hardening steels (closest grade 14NiCrMo13-4 / 1.6657; composition not identical)

A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.

07Is there a better material?

Grades in the same material family as 16NiCrMo12 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than 16NiCrMo12 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

08Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Peeled bar
  • Ground shafting
  • Hexagon
  • Flat bar
  • Plate
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, mechanical tests)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Tensile and impact (Charpy KV) test report
  • Jominy end-quench test (EN ISO 642) report
  • Ultrasonic testing (e.g. EN 10308 for bars, EN 10228-3 for forgings)

Supply status: Available on Request

Request 16NiCrMo12 Quotation

Not sure if 16NiCrMo12 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote