Skip to content

31CrMo12 Nitriding Steel

1.8515

  • EN1.8515
  • EN31CrMo12

Aluminium-free nitriding steel with about 3 % chromium, supplied quenched and tempered. Nitriding gives an 800–900 HV surface while the nitrided layer stays tough; used for extruder screws, plastic mould components and hydraulic pistons.

Spectral Analysis

wt. % · EN 10085 ranges
C
0.28–0.35
Si
≤0.40
Mn
0.40–0.70
Cr
2.80–3.30
Mo
0.30–0.50

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • 800–900 HV surface after nitriding
  • Tough nitrided layer (aluminium-free)
  • Good core strength (Rm 1000–1200 MPa)
  • Low nitriding distortion
  • Dimensional stability at elevated temperature
  • Good machinability in QT condition

02Applications

  • Extruder screws and barrels
  • Nitrided plastic mold components
  • Gears and camshafts
  • Hydraulic pistons and guides
  • Wear-loaded machine elements

03Delivery Condition

  • Quenched and tempered (+QT), ≈ 300–350 HB; peeled / ground bar.

04Heat Treatment

Heat Treatment Steps

HardeningTemperatureTime →Austenitise~900 °C
TemperingTemperatureTime →870–930 °C
NitridingTemperatureTime →500–530 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 52 HRC200 °C → 49 HRC300 °C → 46 HRC400 °C → 43 HRC500 °C → 39 HRC550 °C → 36 HRC600 °C → 33 HRC650 °C → 30 HRC01002003004005006007002530354045505560Tempering temperature [°C]Hardness [HRC]
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 31CrMo12 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Peeled bar
  • Ground shafting
  • Hexagon
  • Flat bar
  • Plate
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, mechanical tests)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Tensile and impact (Charpy KV) test report
  • Jominy end-quench test (EN ISO 642) report
  • Ultrasonic testing (e.g. EN 10308 for bars, EN 10228-3 for forgings)
Request 31CrMo12 Quotation

Not sure if 31CrMo12 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote