Skip to content

17-7 PH Precipitation-Hardening Stainless Steel

1.4568 (17-7 PH)

  • EN1.4568
  • ENX7CrNiAl17-7
  • AISI631 / 17-7 PH
  • UNSS17700
  • AMS5528 / 5529

Semi-austenitic, aluminium-bearing PH stainless steel. Formed in the solution-treated Condition A and then aged to reach tensile strengths of 1300–1650 MPa; used for springs, diaphragms, bellows and thin aerospace sheet.

Spectral Analysis

wt. % · EN 10088-3 / AMS ranges
C
≤0.09
Si
≤0.70
Mn
≤1.00
Cr
16.0–18.0
Ni
6.50–7.80
Al
0.70–1.50

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Soft and formable as delivered
  • Rm 1300–1650 MPa after ageing
  • Good corrosion resistance (304 level)
  • High fatigue strength
  • Low distortion (low-temperature ageing)
  • Common in sheet, strip and wire

02Applications

  • Springs and spring contacts
  • Diaphragms and bellows
  • Aerospace structural sheet parts
  • Pressure vessels and fasteners
  • Surgical and instrumentation parts

03Delivery Condition

  • Condition A (solution treated), ≈ 85 HRB; sheet, strip, wire, bar. Aged condition on request.

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →~1065 °C
Soft annealingTemperatureTime →~760 °C
AgeingTemperatureTime →~565 °C
Stages and temperatures are typical values; soaking times depend on section size.

Ageing Diagram

480 °C → 48 HRC510 °C → 46 HRC540 °C → 44 HRC565 °C → 42 HRC595 °C → 39 HRC620 °C → 36 HRC0100200300400500600700303540455055Ageing temperature [°C]Hardness [HRC]
Hardness versus ageing temperature after conditioning at 760 °C (approximate).

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 17-7 PH with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet
  • Forgings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. EN 10308, ASTM A388), upon request
  • Intergranular corrosion testing (e.g. ASTM A262, EN ISO 3651-2)
  • Detrimental phase testing for duplex steels (ASTM A923)
Request 17-7 PH Quotation

Not sure if 17-7 PH is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.