420 (X30Cr13) Martensitic Stainless Steel
1.4028
- EN1.4028
- ENX30Cr13
- AISI420
- UNSS42000
Martensitic stainless grade with 0.26–0.35% carbon and 12–14% chromium, reaching 48–54 HRC after heat treatment, harder than 1.4021. Used for knives, valve stems and needles, pump shafts and surgical instruments.
Spectral Analysis
wt. % · EN 10088-3 ranges- C
- 0.26–0.35
- Si
- ≤1.00
- Mn
- ≤1.50
- Cr
- 12.0–14.0
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- 48–54 HRC by heat treatment
- Good corrosion resistance (polished, QT)
- Good wear resistance
- Magnetic
- Good machinability annealed
- Limited weldability
02Applications
- Knives and cutting tools
- Valve stems, needles and seats
- Pump shafts and parts
- Surgical and dental instruments
- Plastic mold parts (low volume)
03Delivery Condition
- Soft annealed (+A), max. 245 HB; peeled / ground bar, plate.
04Heat Treatment
Heat Treatment Steps
Quench: Oil, pressurised gas in vacuum or air (thin sections)
Tempering Diagram
Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.
05Is there a better material?
Grades in the same material family as 420 (X30Cr13) with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
- 440B Stainless Steel
Wear resistance: Medium → High
- 440C Stainless Steel
Wear resistance: Medium → High
Higher impact resistance (toughness)
- 420 Stainless Steel
Toughness: Low → Medium
Trade-off: Hardness, Corrosion resistance
- 431 Stainless Steel
Toughness: Low → Medium
Trade-off: Hardness, Wear resistance
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights06Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Flat bar
- Plate
- Sheet
- Forgings
- Cut-to-size
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 inspection certificate (upon request, third party)
- Ultrasonic testing (e.g. EN 10308, ASTM A388), upon request
- Intergranular corrosion testing (e.g. ASTM A262, EN ISO 3651-2)
- Detrimental phase testing for duplex steels (ASTM A923)
Not sure if 420 (X30Cr13) is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialTechnical resources for this material
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.